Post
by eljefe » Tue Nov 02, 2010 6:26 pm
As Cottage cheese puts it succintly:
"...Ok, not to insult the intelligence of the pros on the forum already experienced in such
matters, any newbie attempting phosphate finishing musn't forget the importance of surface
prep... it can't be stressed enough- and no bare hands! The part going into the solution
must be absolutely clean and free of any grease..."
Also, try: finishing.com
the 60ml Nitric acid + 40ml Hcl cold rust method is easy, relatively safe, but will require carding/grinding wheel and buffing etc.
try on waste metal FIRST.
IFG does not offer any liability, implied or otherwise , for information posted on this website.
''It dont mean a thing, if it aint got that zing!''
"...Oh but if I went 'round sayin' I was Emperor, just because some moistened bint lobbed a scimitar at me, they'd put me away..."